Skip to content

Hot Punch Square Hammer Drift for Blacksmiting 2.2 lbs

$158.00 Regular price
🙌 Just available
Engraving:

Hot Punch Square Hammer Drift for Blacksmiting 2.2 lbs

  • Blacksmith Tools Mastery: Elevate your craft with our 2.2lbs Hot Punch Square Hammer Drift, specifically designed to ensure precision and durability for blacksmithing professionals and enthusiasts alike.
  • Durable Blacksmithing Tool: Crafted to perfection, the head of our hammer drift is forged from high-quality C 70W2 steel and exhibits an impressive hardness level of Rockwell 48-52(HRC), promising resilience and longevity even with regular, robust use.
  • Expertly Designed Square Hammer Drift: With an overall length of 13.77" and a 6.3" head size, this tool is optimally sized for control and maneuverability, ensuring each strike is accurate and effective in your blacksmithing projects.
  • Personalized Hot Punch Hammer: Stand out with our customizable hand-forged hammer! Opt for a personal touch with our engraving services, allowing for text or logo to be artfully inscribed on the ashwood handle, making your tool uniquely yours.
  • Hand-Forged & High-Quality Eye Drift: Experience the difference of a carefully hand-forged hammer drift, ensuring each piece is unique, top-quality, and built to last, becoming an essential part of your blacksmith hammer collection and creations.

Technical Details:

Overall length: 13.77" (350mm)
Overall weight: 2.2lbs (1kg)
Head size: 6.3" (160mm)
Hardness: Rockwell 48-52(HRC)
The material of the head: forged from C 70W2 steel, hardened and tempered
Handle material: ashwood
Engraving: we can make your personal engraving on the wooden part of the handle: text, logo

HOW WE DO

Hardening:
We preheat the hammer to about 1200°F (649°C).
Then we increase the temperature to 1450°F to 1500°F (788°C to 816°C).
Quench the hammer in the water.
Tempering:
To reduce the brittleness and increase toughness, tempering is essential.
We clean the surface of the hammer to expose bare metal. This helps in monitoring the tempering colours.
We heat the hammer in an oven. Aim for a temperature between 400°F to 500°F (trying to get 225°C) for a good balance of hardness and toughness.
W hold the temperature for at least an hour per inch of thickness.
Then we allow the hammer to cool to room temperature.
Testing and Verification:
After tempering, we test the hammer's hardness using a Rockwell hardness tester.
Also, we have a simple rebound test. we strike the hammer against an anvil; it should rebound without chipping or deforming.

SKU: ykhamm-8
Hot Punch Square Hammer Drift for Blacksmiting 2.2 lbs from AncientSmithy
Hot Punch Square Hammer Drift for Blacksmiting 2.2 lbs $158.00 Regular price

Need help?

Frequently Asked Questions